Advertising Signs
ADS-MX2 Laser pulsed spot welder
This equipment is specifically designed for the advertising lettering industry, as well as for thin-gauge sheet metal parts such as cabinets, niches, and water tanks.
Product Details
Product Positioning
This equipment is specifically designed for the advertising lettering industry, as well as for thin-gauge sheet metal parts such as cabinets, niches, and water tanks. It utilizes a quasi-continuous wave (QCW) fiber laser to produce high-peak-power, narrow-pulse-width laser pulses, perfectly addressing the challenges of spot welding thin sheets of stainless steel, titanium alloys, and coated metals with thicknesses ranging from 0.3 to 2.5 mm.
Key Features
1. Minimal thermal deformation—controlled within 0.3–1.0 mm
Principle: In pulse output mode, each pulse acts for an extremely short duration (millisecond level). Heat is rapidly concentrated on the material and then quickly dissipated, resulting in a heat-affected zone that is only 1/3 to 1/5 the size of that produced by traditional continuous laser welding.
Results: When welding thin sheet metal parts such as stainless steel lettering borders, cabinet panels, and niche frames, the workpieces exhibit virtually no warping or shrinkage, eliminating the need for subsequent flattening.
2. No post-welding treatment required—particularly suitable for coated/colored sheets
Titanium alloy sheets, color-treated stainless steel sheets, galvanized/nickel-plated sheets: The highly concentrated pulse laser energy does not damage surface coatings or baked-on paint; the back of the weld shows no burn marks or oxidation discoloration.
Thin stainless steel sheets: The weld appears silvery-white or pale yellow, requiring no grinding, acid washing, or polishing before proceeding directly to the next process.
3. Welding Efficiency Increased by 2–3 Times
Compared to traditional TIG spot welding, a pulsed spot welder requires only 0.2–0.5 seconds per spot and does not require filler wire.
Compared to continuous laser welding, the pulsed mode eliminates the need for complex oscillation during spot welding of thin sheets, resulting in faster speeds. It is particularly suitable for high-density spot welding operations such as the edging of advertising letters and water tank reinforcing ribs.
4. Aesthetically Pleasing and Strong Welds
With stable pulse energy, the weld spots are smooth, uniform in size, and free of spatter and porosity.
Shear strength can reach over 85% of the base material’s strength, meeting structural strength requirements.
Welding Parameters
Serial number | Project name | Parameters |
1 | Central wavelength | 1080nm+5nm |
2 | Output peak power | 1500W |
3 | Working mode | continuous/pulse |
4 | Polarization direction | random |
5 | Maximum average power | 750W |
6 | Maximum continuous power | 1000W |
7 | Repetition frequency | 0-1000Hz |
8 | Pulse width | 0.5-50ms |
9 | Maximum single pulse energy | 75J |
10 | Output power instability | 3% |
11 | Output header form | OBH |
12 | Fiber core diameter | 200/360ym |
13 | Numerical aperture | 0.22 |
14 | Fiber length | 10m |
15 | Indicating light | 650nm 0.3mw~lmW |
16 | Working voltage | AC 220V+10%, 50/60Hz |
17 | Maximum power consumption | 2200W |
18 | Control method | RS232 |
19 | Appearance size | 353*463*123mm |
20 | Weight | ≤38kg |
21 | Working environment | Temperature 5~40℃, humidity <65% |
22 | Storage environment | -10~60℃ |
23 | Cooling method | air cooling |
Suitable For Industry
Delivery & Shipping Arrangements
Orders placed on the official website are shipped from headquarters.
In-stock items are shipped within 3–15 business days of payment; items not in stock are typically shipped within 25 business days.
If the goods are unsuitable for standard shipping methods, or in other special circumstances, please notify us in advance so that a solution can be mutually agreed upon.
Consult Now
Please enter your contact information, and we will get in touch with you as soon as possible.
Related Products